Our special design and composition pot wheel, which we have developed for grinding the surface of rails and their weld seams. Our wide range of raw materials ensures that different compositions of rails are efficiently machined.
Binding: Bakelite
Shape 6
Cylindrical pot-shaped grinding wheel
DxTxH-W..E..

| Dimensions | ||||||
| D | T | H | W | E | Cutting speed m/s | |
| 50 | 50 | 20 | 10 | 10 | 35 | |
| 60 | 40 | 20 | 10 | 10 | 32 | |
| 75 | 50 | 32 | 8,5 | 10 | 35 | |
| 80 | 30 | 20 | 12 | 10 | 32 | |
| 80 | 50 | 20 | 10 | 10 | 25 | |
| 100 | 60 | 51 | 4,5 | 15 | 32 | |
| 100 | 85 | 20 | 24 | 25 | 50 | |
| 100 | 80 | 51 | 18,7 | 20 | 50 | |
| 100 | 110 | 22 | 17 | 20 | ||
| 100 | 110 | 22 | 18,7 | 20 | 50 | |
| 125 | 45 | 16 | 10 | 10 | 32 | |
| 125 | 63 | 20 | 6 | 13 | 35 | |
| 125 | 100 | 20 | 20 | 16 | 35 | |
| 160 | 80 | 22,2 | 20 | 20 | 25 | |
| 175 | 75 | 76 | 15 | 15 | 35 | |
| 175 | 100 | 76 | 15 | 15 | 35 | |
| 200 | 100 | 76 | 30 | 25 | 35 | |
The cutting speed depends on the other characteristics of the grinding wheel: 32 / 35 / 40 / 45 / 50 (m/s).
For efficient machining of individual materials grades, ask our technology consultants or technical sales representatives for an offer.